Thermal oxidation of poly(Dicyclopentadiene) – Decomposition of hydroperoxides ArchiMer
Huang, Jing; Minne, Wendy; Drozdzak, Renata; Recher, Gilles; Le Gac, Pierre Yves; Richaud, Emmanuel.
Thin unstabilized PDCPD film were thermally oxidized in ovens at several temperatures ranging from 50 °C to 120 °C. Hydroperoxide concentration was monitored by DSC. It was observed that hydroperoxides concentration reaches a plateau with short induction times, for example around 8 h at 50 °C. This plateau occurs at very high concentration, around about 1 mol l−1 at 50 °C. In order to study both the chemical mechanisms and the kinetics of hydroperoxides decomposition, oxidized samples were thermally aged in an inert atmosphere to destroy hydroperoxides. For initially high concentrations corresponding to the “plateau”, it was shown that hydroperoxides decompose following a bimolecular process, the rate constant of which being calculated from the...
Tipo: Text Palavras-chave: Polydicyclopentadiene; Thermal oxidation; Hydroperoxide decomposition; Polymerization catalysts.
Ano: 2020 URL: https://archimer.ifremer.fr/doc/00609/72080/70798.pdf
Registros recuperados: 1
Primeira ... 1 ... Última
 

Empresa Brasileira de Pesquisa Agropecuária - Embrapa
Todos os direitos reservados, conforme Lei n° 9.610
Política de Privacidade
Área restrita

Embrapa
Parque Estação Biológica - PqEB s/n°
Brasília, DF - Brasil - CEP 70770-901
Fone: (61) 3448-4433 - Fax: (61) 3448-4890 / 3448-4891 SAC: https://www.embrapa.br/fale-conosco

Valid HTML 4.01 Transitional